Dear MPK

Yes

SS & CS filler wire comes under F No 6
Material Qualification range: P1-to P15F P34, P41-P49 if qualifies in
any one of this,
So it covers material range.
deletion of purging is a essential variable for WQT
so welder qualifies for both if qualifies in CS
This as per the Code

But it is better to set the internal standard by firm to qualify
welders for SS separately considering the practical difficulties in
Welding

regards
Samshuddin.K
NKOM
regards
Samshuddin.K


On 3/22/12, mpk mpk <ranmi2007@gmail.com> wrote:
> Dear Experts,
>
> If a welder is qualified in CS - GTAW process, Is the same welder can weld
> SS - GTAW process with purging ?
>
> Thank you,
> MPK
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...