Wednesday, March 21, 2012

Re: [MW:13965] TENSILE TEST REQUIRMENT FOR PLATES AFTER SIMULATION HEAT TREATMENT

Dear Mr. Asad,
 
Please refer S3 and Clause No. 11 of SA 20.
 
With regards,
 
 
C. R. GANDHI
(Manager- Q. A.)

--- On Wed, 3/21/12, asad azmi <azmiasadayub@gmail.com> wrote:

From: asad azmi <azmiasadayub@gmail.com>
Subject: [MW:13963] TENSILE TEST REQUIRMENT FOR PLATES AFTER SIMULATION HEAT TREATMENT
To: materials-welding@googlegroups.com
Date: Wednesday, March 21, 2012, 4:56 PM

Dear All,
 
A vessel is being fabricated as per ASME SEC VIII DIV 1.
 
 
Contarctor has received 3 plates ( SA 516 GR 70 N - 30 mm Thk) which are having one heat number and 3 different Plate No. Plate condition - Plate Hot Rolled. plate manufacturer has not done Simulation heat treatment of test coupon.
 
as per Client  Simulation  heat treatment ( 3 pwht cycle) is reuired. 
 
As per SA 20 PARA 11.1.1 One tension test is required for each plate as rolled. as per client requirment any mechanical testing shall be done after all heat treatment.
 
 
Please advice whether one sample from each plate has to undergo simulation heat treatment cycle & Tension test OR one sample out of any 3 plates shall undego simulation heat treatment & Tension Test.( as heat number is same for each 3 plates)
 
Please give code reference.
 
Thanks & Regards
 
Asad Azmi
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...