Hi

Temporary Blind flanges thickness may be layered to meet the hydrotest
pressure thickness. However, the welding of both plates shall be layered as
per ULW-17(g) and fig ULW 17.4 of ASME Sec VIII, Div.1.

BR
M.Vijayan


-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of veera raghava
kommisetti
Sent: Wednesday, March 21, 2012 9:02 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:13958] REQUIRMENT FOR TEMPORARY BLIND FLANGE USED FOR
HYDROTEST

When two plates are welded, which means only welded at edges.
so there is chance of are gap between the plates else where, which is
effectively single plate thk. (If lamination exisit at 50mm depth on
100 mm plate then effective thk is only 50mm). same logic applies.


On 3/20/12, prasad rao <prasadrao31@gmail.com> wrote:
> Can you Brief us in what way it is unsafe and dangerous .
>
> As per the above photograph it is totally welded so there is no risk
> in that .But it not Good practise you say.
>
> --
> To post to this group, send email to
> materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views
> and meant for educational purposes only, Users must take their own
> decisions w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.

This communication and any files transmitted with it are confidential and may also be privileged. It is for the exclusive use of the intended recipient(s). If you are not the intended recipient or the person responsible for delivering it to the intended recipient(s), please note that any form of distribution, copying or use of this communication or information contained in it is strictly prohibited and may be unlawful. If you have received this communication in error please return it to the sender, and delete the material from any computer. We reserve the right to monitor email communications through normal internal and external networks. We believe but not warrant that the email and the attachments are virus free. The statement and opinions expressed in this communication are those of the writer and do not necessarily represent those of Madina Group, whose registered office address is

P.O. Box 20459, Doha, Qatar.
Tel. +974 44600818
Fax. +974 44603143

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...