Wednesday, March 21, 2012

Re: [MW:13958] REQUIRMENT FOR TEMPORARY BLIND FLANGE USED FOR HYDROTEST

When two plates are welded, which means only welded at edges.
so there is chance of are gap between the plates else where, which is
effectively single plate thk. (If lamination exisit at 50mm depth on
100 mm plate then effective thk is only 50mm). same logic applies.


On 3/20/12, prasad rao <prasadrao31@gmail.com> wrote:
> Can you Brief us in what way it is unsafe and dangerous .
>
> As per the above photograph it is totally welded so there is no risk in
> that .But it not Good practise you say.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...