Re: [MW:13952] REQUIRMENT FOR TEMPORARY BLIND FLANGE USED FOR HYDROTEST

It is not safe.Could be dangerous.
Regards
aarpee

On Tue, Mar 20, 2012 at 4:48 PM, asad azmi <azmiasadayub@gmail.com> wrote:
Dear All,
 
A vessel is being fabricated as per ASME SEC VIII DIV 1.
 
A temporary blind flange fabricated from plate is used for hydrotest. Hydrotest pressure is 3003 PSIG.
 
During hydrotest it was observed that contractor has welded two plates to obtain required thcikness for temporary blind flange.Please refer attached photo.
 
Whether practise of acheving required thickness of blind flange by welding 2 or more plate is safe and acceptable.
 
please give code reference.
 
Thanks & Reagrds
 
Asad Azmi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...