[MW:14026] Re: PWHT OF P91 BY INDUCTION HEATING

Dear Pradip Sir,

Thank you very much for valueble informations. We are going to conduct
another PWHT mock test,considering all these facts and skilled
technicians have been called for the same.

Regards,


Sandeep
Qc Engineer

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...