Wednesday, March 28, 2012

[MW:14009] Re: Speed of Tensile Test

Normally Steady & uniform Load application during the tensile test is
necessary, the speed of the tensile test is not mandatory according to
my knowledge but high rate of loading is avoided.

On Mar 28, 4:39 pm, Pushpraj Anand <pushprajanan...@gmail.com> wrote:
> What is the speed of tensile test for Procedure qualification as per section IX?
>
> i read some coads they recommended for some speed of tensile test,is
> it mandatory to follow or we can do at any speed?
> --
> Regards,
> Pushpraj Anand

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...