[MW:14008] RE: 13998] Can SMAW welders qualified in matl Grade A36 weld also S355 ..ASME section IX

Only if you can meet the requirements of QW-423.1 and QW-423.2 for
unlisted materials similar to listed materials. I have found it is
generally a tough sell to customers.

John A. Henning
Welding & Materials

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Anthony
Sent: Tuesday, March 27, 2012 1:20 AM
To: Materials & Welding
Subject: [MW:13998] Can SMAW welders qualified in matl Grade A36 weld
also S355 ..ASME section IX

we generally have welders qualified to A36 in our firm as per sec
presently we are working on a project demanding S355 JR /JO and we have
qualified the procedure and wleders also but can i use my other welders
who are qualified in A36[3G] and A106 Gr B [6G] as per ASME sec IX

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.

______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...