[MW:13972] FW: 13970] Filler for Monel to carbon steel

Use ERNiCu-7 ….. It can also be used for joining these alloys to steel. usually welded with pure Ar as the shielding gas.

 

 

Eng. Ahmed Osman

Senior QA/QC Eng.

Orascom Construction Egypt

+20 122 5880434

ahmed.mahmoudmohamed@orascomci.com

a.osman81@yahoo.ca

 

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Dsunil
Sent: Thursday, March 22, 2012 7:28 PM
To: materials-welding@googlegroups.com
Subject: [MW:13970] Filler for Monel to carbon steel

 

Dear Experts,

 

Can  you recommend the filler in ER series  for welding  Monel 400  to  Carbon Steel (A105)  material.

 

Thanks and regards

S G Dixit

Sr. Manager- Materials

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...