Thursday, February 2, 2012

Re: [MW:13598] use ER316L to weld A312 TP 321

No, you need to use E/ER 347 to obtain optimal properties and good weld joint.
 
If Impact test is not applicable, then you can use the 316L PQR and prepare a WPS with E347 as the electrode.
 
Thanks & Regards J.Gerald Jayakumar 0091-9344954677
From: Mohamed Elsayed ( BTG) <MElsayed@ccc.ae>
To: materials-welding@googlegroups.com
Sent: Thursday, February 2, 2012 11:09 AM
Subject: [MW:13597] use ER316L to weld A312 TP 321

Gents,
I need your valuable advice on following.
 
We have some joints in for Flare package ,
 
Can we use ER316L filler wire to weld
1-      butt welded joints A312 TP 321
2-      Butt welded Joints A403 WP 321
 
Separatly ,
 
We have  supporting PQR USING ER316L  welded material  A240 316L , can this PQR suppot welding
1-      butt welded joints A312 TP 321
2-      Butt welded Joints A403 WP 321
 
Waitting your reply ASAP
 
Thanks
Mohamed
 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

[MW:35346] Cast-iron welding

Any advice for cast iron welding Sent from Yahoo Mail for iPhone