Can someone explain me following ASME clause regarding thickness range qualified by welder & is it OK if a welder welds 13 mm & above with 3 or more layers, he is qualified for maximum thickness ( e.g. 50mm or more )

 

 

 

 

 

 

 

 

 

Best Regards,

Vivek Jadhav

 

No comments:

Re: [MW:35686] HDPE WPS