Dear experts,
Need your help on this issue urgently...
We have a heavy vessel thick with construction code ASME Sec-VIII div.2 and lethal service.
The plate materials SA-516 Gr.60/70N are exempted from impact testing but SRF fogings as per the thickness requirements need impact testing.
Does this means that the joint made between SRF nozzle & Shell shall require an impact test WPS.
Also as we know that the production test coupons (PTC) are required only for A & B category joints, where as Shell to SRF Nozzles fall in D category weld joint, will it call for PTC's.

Waiting for reply...

Shadab Ansari

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...