I have PQR qualified for Alloy 825 welded with E NiCrMo3. I need
weld C 276 to C276. The recommended filler wire fir the same is E
NiCrMo4.
What are the effects if i welded C 276 with ENiCrMO3. Can i use
Alloy 825 PQR for C 276.
Regards
VENKAT
--