Hi
Keep the IQI on film side and place letter “F” in the film.
BR
M.Vijayan
From: vijayan [mailto:vijayan.m@madinagulf.com]
Sent: Wednesday, January 11, 2012 4:06 PM
To: 'materials-welding@googlegroups.com'
Subject: RE: [MW:13448] RE: 13441] NDE FOR BUTT WELD
Hi
Can you try as per the attached sketch.
Keep hole type IQI. Don’t bend the film cassette. Go for touching shot. I think you will get good result.
Pls update once done!
BR
M.Vijayan
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Desai Jignesh (Mumbai - Piping)
Sent: Tuesday, January 10, 2012 3:37 PM
To: materials-welding@googlegroups.com
Subject: RE: [MW:13448] RE: 13441] NDE FOR BUTT WELD
It is a butt weld.
It is welding of SS 321 forged component (Nozzle) of bevel end with 90 el. Actually forged nozzle is without tapering.
Proper radiography is executed for the BW valves joints as shown in Photo-0060.
UT is also a problem since probe movement is possible at only one side (Towards elbow) and there is no inside access.
It is 100% Radiography lines with high pressure – 1500#.
Regds/Jignesh
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of vijayan
Sent: 10 January 2012 16:18
To: materials-welding@googlegroups.com
Subject: [MW:13444] RE: 13441] NDE FOR BUTT WELD
Hi
What is the joint configuration
BR
M.Vijayan
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Desai Jignesh (Mumbai - Piping)
Sent: Tuesday, January 10, 2012 12:58 PM
To: materials-welding@googlegroups.com
Subject: [MW:13441] NDE FOR BUTT WELD
Can somebody write me about the possibility of either radiography OR Ultrasonic testing of attached butt weld?
We have tried to carry out radiography with and without non metallic support as in the attached snaps but image is not clear.
Regds/Jignesh
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
This communication and any files transmitted with it are confidential and may also be privileged. It is for the exclusive use of the intended recipient(s). If you are not the intended recipient or the person responsible for delivering it to the intended recipient(s), please note that any form of distribution, copying or use of this communication or information contained in it is strictly prohibited and may be unlawful. If you have received this communication in error please return it to the sender, and delete the material from any computer. We reserve the right to monitor email communications through normal internal and external networks. We believe but not warrant that the email and the attachments are virus free. The statement and opinions expressed in this communication are those of the writer and do not necessarily represent those of Madina Group, whose registered office address is
P.O. Box 20459, Doha, Qatar.
Tel. +974 44600818
Fax. +974 44603143
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
This communication and any files transmitted with it are confidential and may also be privileged. It is for the exclusive use of the intended recipient(s). If you are not the intended recipient or the person responsible for delivering it to the intended recipient(s), please note that any form of distribution, copying or use of this communication or information contained in it is strictly prohibited and may be unlawful. If you have received this communication in error please return it to the sender, and delete the material from any computer. We reserve the right to monitor email communications through normal internal and external networks. We believe but not warrant that the email and the attachments are virus free. The statement and opinions expressed in this communication are those of the writer and do not necessarily represent those of Madina Group, whose registered office address is
P.O. Box 20459, Doha, Qatar.
Tel. +974 44600818
Fax. +974 44603143
No comments:
Post a Comment