Re: [MW:12108] welding position limitations for SMAW & GTAW

Dear A. J. Khan,

Find the attached file. Hope it will help you.

Also, the position limits is applicable to all types of welding not only SMAW or TIG.

Nandeesh

--- On Wed, 3/8/11, abdul khan <abdul_khan2010@yahoo.co.in> wrote:

From: abdul khan <abdul_khan2010@yahoo.co.in>
Subject: [MW:12096] welding position limitations for SMAW & GTAW
To: materials-welding@googlegroups.com
Date: Wednesday, 3 August, 2011, 6:25 PM

Dear Experts ,
 
can any one say The welding postioin  limitations for SMAW & GTAW .
 
It will be appriciated  if you mention  reff Standard.
 
Waiting for Reply from weldiing Experts .
 
Regards.
ABDUL JABBAR KHAN

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...