Re: [MW:12109] 0.2% offset method

Hi,
 
generally it is not possible to determine yeild strength, so it is generally accepted that the stress which creates 0.2% elongation will be yeild stress.
 
Regards
Manpreet Singh
 


From: prashant pansare <prashantpan_99@yahoo.co.in>
Sent: Thu, 04 Aug 2011 09:39:56
To: mat wel <materials-welding@googlegroups.com>
Subject: [MW:12066] 0.2% offset method
Dear All,
In some of the materials we need to go for 0.2% offset method for Y.S. Why?
& 0.2% of which value is to be calculated?
Thanx & Regds,
PSP

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Treat yourself at a restaurant, spa, resort and much more with Rediff Deal ho jaye!

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...