Monday, August 1, 2011

Re: [MW:12032] Single bevel PQR can we use as backweld

Dear Mr. Bharat,


We had the same issue during our ASME audit (it was our first U-stamp audit).There is no problem in using the 
above PQR for making a procedure with full E7018 electrode provided backwelding should be done. 

As the E7018 with F4 we used in the PQR we are not violating the re

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...