Monday, August 1, 2011

Re: [MW:12033] Minimum distance between butt weld joint and support weld

Dear Raj,
Maintain 50 mm (or) 4 times the pipe wall thick
which ever is less.
there is no data in the code reg this.
Regards
Mano

2011/7/31, ratna sekhar <badderaj@yahoo.co.in>:
> Dear experts,
> Can any one please confirm the Minimum distance between butt
> weld joint and support weld.
> And where that data will be available.
> Regards,
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...