Hi,
I also came to same conclusion but still not  conveinenced fully myself....
Expecting comments from other experts too...
Regards
Bharat


 

Date: Sun, 31 Jul 2011 20:52:39 +0530
From: abdul_khan2010@yahoo.co.in
Subject: Re: [MW:12014] Single bevel PQR can we use as backweld
To: materials-welding@googlegroups.com

Dear Bharat,
 
The F.No for E7018  is 4
 
The F.No for E6010 is 3
 
Hence Change in F Number is Essential Variable. For change in Essential Variable Requalification of PQR is Required. you cant make WPS for E7018 only. 
 
Hope the answer to your question .
 
Regards
 
Abdul Jabbar Khan


--- On Sun, 31/7/11, BHARAT GOLE <bharatgole@hotmail.com> wrote:

From: BHARAT GOLE <bharatgole@hotmail.com>
Subject: [MW:12003] Single bevel PQR can we use as backweld
To: "Material Welding" <materials-welding@googlegroups.com>
Date: Sunday, 31 July, 2011, 4:54 PM

 I have PQR with for single bevel with E6010 root & E7018 for fill & Cap as per ASME IX
Can I prepare WPS with back weld with help of same PQR.....only using E7018 ?
Expert your comments pl with ref to ASME Clause
Regards
Bharat


 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...