Re: [MW:11986] DOT/DWT qualification

If in your case, conditions require simultaneous operation where one welder may affect another welder, I believe you want to go for a WQT (not PQR) with the same conditions.

However if the job is like welding a pipe and welders are already qualified, that doesn't need a new qualification.

It's up to your judgement...!!!

Ramin  Kondori
   QC/Welding Engineer 
         IWE AT 0070
   



On Fri, Jul 29, 2011 at 7:51 PM, abdul khan <abdul_khan2010@yahoo.co.in> wrote:
Dear Prasu,
 

The simple answer read it carefully.

 

Essential variable: The variable which affects the properties of the weld metal is known as essential variable. Change in essential variable requires requalification of PQR.

 

Welding Technique is Non essential variable and hence will not affect the properties of the weld metal and no requalification of PQR is required.

 

The DOT/DWT technique it will not affect the properties of the weld metal and hence Requalification of PQR is not required nor the welders Requalification required if welders are qualified for suitable position and thickness range of base metal.

AS PER MY KNOWLEDGE

 

Hope the answer to the question

 

Regards

ABDUL JABBAR KHAN  

 
normally for requalification of PQR the
--- On Fri, 29/7/11, Prasu Cutie <pracuty@gmail.com> wrote:

From: Prasu Cutie <pracuty@gmail.com>
Subject: [MW:11976] DOT/DWT qualification
To: materials-welding@googlegroups.com
Date: Friday, 29 July, 2011, 4:57 PM


Dear Experts,
Is welder qualification & PQR qualification is required for DOT/DWT technique????? *(As per Sec.IX)

DOT-- Double operator technique
DWT-- Double welder technique

Awaiting for reply!!!!!!!!!

Regards
prasu
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...