You have to bearin mind the cost of Ti which is very very costly


From: vijay <vijayakumarme@gmail.com>
To: materials-welding@googlegroups.com; weldinggang@googlegroups.com
Sent: Thu, 14 April, 2011 5:25:58 AM
Subject: Re: [MW:10669] Titanium to carbon steel welding

Dear  Schreedhar/ Rizal/ Shaunak Upadhyay / Prakash Hegde,

Thanks for your valuable suggestions.
The saddle length is 200mm only, and I have suggested to use Titanium for the saddle to avoid dissimilar welding.
I think this will be the better decision to avoid carbonsteel to titanium welding problem.

Thanks and Regards,
Vijay



,

On Tue, Apr 12, 2011 at 1:06 PM, Prakash Hegde <pb.hegde@yahoo.com> wrote:
Dear Vijay
 
Ti To  Cs welding is not compatable
Generally  Ti lining (sheet ) is being screwed with CS, You  can refer AWS welding Hand book Vol 4 for the joint configuration Which will  clear your doubts
Regards
 
Hegde P.B.


From: vijay <vijayakumarme@gmail.com>
To: weldinggang@googlegroups.com; materials-welding@googlegroups.com
Sent: Tue, 12 April, 2011 6:09:13 AM
Subject: [MW:10646] Titanium to carbon steel welding

Dear Friends,

There is a requirement mentioned in our client spec about Titanium to Carbon steel welding(Attached picture have more details).
I searched for literatures on this and I found that by normal fusion welding process is not recommended.
1. Is there any way,welding can be done between Titanium and carbon steel?
2. If YES or NO(on both case), please send a evidence document to confirm(like ASME,ASTM).
This is very urgent requirement.

Thanks in advance

Regards,
Vijay

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...