Re: [MW:10648] Titanium to carbon steel welding

Dear Vijay,

There is no any consumable or process to join titanium to carbon steel welding.

Please give your joint details and materials specification for other details.

On Tue, Apr 12, 2011 at 6:09 AM, vijay <vijayakumarme@gmail.com> wrote:
Dear Friends,

There is a requirement mentioned in our client spec about Titanium to Carbon steel welding(Attached picture have more details).
I searched for literatures on this and I found that by normal fusion welding process is not recommended.
1. Is there any way,welding can be done between Titanium and carbon steel?
2. If YES or NO(on both case), please send a evidence document to confirm(like ASME,ASTM).
This is very urgent requirement.

Thanks in advance

Regards,
Vijay

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Regards,
Shaunak Upadhyay,


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...