Monday, April 11, 2011

Re: [MW:10645] Pqr

Hi,
 
If you are qualified the PQR as per ASME Sec-IX, then weld a test coupon as per the old PQR variables and do only hardness as per NACE MR0175 requirements.
 
Please refer QW-401.3, though it is mentioned for supp essential variables, you can approach your client for the deviation.
 
Also please read the following Sec-IX interpretations.
 

Interpretation: IX-07-08

Subject:            QW-200.2(c), Changes to PQR (2007 Edition)

Date Issued:     February 12, 2008

File No:            08-209

 

Question (1):  Can additional tests and data that are not required by Section IX (i.e., hardness

ferrite, corrosion, etc.) be added to a PQR at a later date when the testing was not performed as

part of the original PQR, but followed the conditions of the original qualification?

 

Reply (1):  Yes.

 

Question (2):  If the tests and data noted in Question 1 are added to the PQR, would

recertification, including date, be required?

 

Reply (2):  Yes.  All changes to a PQR require recertification (including date) by the

manufacturer or contractor per QW-200.2(c).

 

 
Cheers!
 
Raj

On Sun, Apr 10, 2011 at 9:09 AM, vijay kumar <vijaykumaar80@gmail.com> wrote:
Thank you for your reply,
 
My Point's is 1) hardness readings taken from 5 locations by old method but nace requirment is 19 locations

2) Need to requalify the hole procedure or only hardness test
 
pls give the advise with code reference
 
 
On Fri, Apr 1, 2011 at 9:49 AM, Engineer Mech <mengineer010@gmail.com> wrote:
Hi,

Method is not a matter,
The values are important,
 if ur old values satisfy with new requirement then no need go for A new PQR.

Tnks



On Thu, Mar 31, 2011 at 3:47 PM, vijay kumar <vijaykumaar80@gmail.com> wrote:
Dear all
 
We have a previous project qualified welding procedure, but hardness test carried out in old method in that pqr, present project spec is saying that requirement of test as per NACE MR0715 ISO 15156. i have some doubts about it
 
we can weld a coupon as per wps and do the hardness test as per nace requirment or need to qualify newly with all tests
pls send the reply with code reference
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...