Mr.Vijay kumar,
 
 you can check API-1104 6.2.2-D For diameter ranges as essential variables
 
as : <2.375,
       From 2.375 to 12.75,
       >12.75
 
 
Regards,
 


 
On Sun, Apr 10, 2011 at 9:15 AM, vijay kumar <vijaykumaar80@gmail.com> wrote:
procedure Qualification as per API 1104 Dia Range Is essential Variable or non?
 
api 1104 5.3.2.3 is showing that need to specify diameters and wall thickness in wps but Essential Variables (5.4) doesn't Say's that dia range
 
waiting for valuable replays
 
thnks

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...