Wednesday, April 6, 2011

Re: [MW:10613] reducing and equal tee modification

Hi there


It appears that it is something more than a mere of a code. I found it in our project technical specification where stated clearly that fabrication of branch connection is not acceptable. Read the entire contents of your project specification to get the answer.


rgds

2011/4/3 Ahmed Eissa <ahmedeissa16@yahoo.com>
dear all.
 
we have reducing tee 2"/1" installed, but we would to install equal tee 2"/2" , due to unavailability , some one has suggisted to cut 1" outlet and to install 2" pipe is it allowed or possible in ASME B31.1 ?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...