Re: [MW:10561] regarding: poldi hardness bar

and it is in BHN (Brinell Hardness No.) From what you say it should be less than that for the bar...

--- On Fri, 1/4/11, muthusrinivasan muthuselvam <msms2k@gmail.com> wrote:

From: muthusrinivasan muthuselvam <msms2k@gmail.com>
Subject: Re: [MW:10558] regarding: poldi hardness bar
To: materials-welding@googlegroups.com
Date: Friday, 1 April, 2011, 1:58 PM

The value you are getting from the conversion table is direct valve no need to multiply....
 
br,
msms

On Thu, Mar 31, 2011 at 6:43 PM, venkat kumar <vsslsrk@gmail.com> wrote:


dear experts,

very good day all of you.

sir's we are checking hardness of pipe.for this purpose we are using poldi hardness tester.every one know that poldi hardness tester having one standard hardness bar and some value given in that bar.we are taking indentation on bar and test specimen ( that means in piping: parent metal,haz1,weld zone,haz2),after taking two indentations and matching in convertion table.for example: we obtained on pipe parent metal 2.0mm indentation and on bar it is 1.9mm.and these both values we checked in convertion table we obtain 222.my question is this reading is briness hardness value or we have to multiply with standard hardness bar value. pl clarify me


thanks & regards





--
thanks & regards


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35346] Cast-iron welding

Any advice for cast iron welding Sent from Yahoo Mail for iPhone