Re: [MW:10551] WELD DETAIL FOR WELDING OF AL 6082-T6

You can use ER4043

Regards,

(Karthik)

On Thu, Mar 31, 2011 at 6:43 PM, Martin Prad <martin_prad@hotmail.com> wrote:
Dear Friends,
 
Could you please advise some details (welding consumable+elecrtricial detail) for welding of aluminum grade 6082-T6?
Your valuable inputs will be highly appreciated.
 
Thanks,
Martin.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...