[MW:10690] RE: 10688] ABS GR, AH-36 MATERIAL

Hello Bhaskar,
 
You may please refer ASTM-A-131-Standard Specification for Structural Steel for Ships. This steel is classified as:-
  • Higher Strength—Grades AH, DH, EH, and FH with a specified minimum yield point of 46 ksi [315 MPa], 51 ksi [350 MPa], or 57 ksi [390 MPa].
Thanks.
 
Pradip Goswami,P.Eng.IWE
Welding & Metallurgical Specialist & Consultant
Ontario,Canada.
Email-pgoswami@sympatico.ca,
 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of bhaskar rao
Sent: Saturday, April 16, 2011 2:54 AM
To: materials-welding@googlegroups.com
Subject: [MW:10688] ABS GR, AH-36 MATERIAL

Dear friends,
 
Please give me the reply for ABS GR,AH-36 Equalent material in
 ASME or ASTM.
 
Regards,
 
PBRAO,

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...