Dear Members,

This is with reference to Normalizing requirement clad dish ends above
16mm Thickness.

Is it advisable to go for Normalizing treatment of clad dish end(300
series clad, Duplex).

As most of the customer ask in the specification that dish end above
16mm shall be normalised, can we interpret this that the same is
applicable for non cladded plates only.

What may be the pros & cons.

Regards

Jaspal Singh
Quality Assurance
ISGEC-Yamunanagar
-9996624244

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...