Dear Sir ,
 
The valve is 8" Ball Valve 600# (trunion type ) but my question is if the valve sustain 7 Kg/Cm2 air pressure then is it possible to sustain 95 kg N2 Pressure . 

 
On 8/17/10, Suresh <bobsuresh24@gmail.com> wrote:
first you need to conirm that what type of valve and what manufacture spec is followed .
 
Depends on Spec , there is mentioned clearly  maximum allowed test pressure according to valve calls,rating,.Hence  It should not be exceeded .
 
Please mentioned full details then we can discuss further
 
Thanks
Suresh

 
On 8/16/10, soumya podder <soumya.podder@gmail.com> wrote:
Dear Sir ,
 
We did pneumatic test of a 600 Class Valve by air at 7 Kg/Cm2 but at site we do by N2 Gas upto 95 Kg/Cm2 , My question is - The pressure of both are same or N2 Pressure is high ?

--
Thanks & Regards

Soumya Podder
9099982514

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks  & Best Regards,

Suresh

Mobile No: 91-92 92 905 905

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks & Regards

Soumya Podder
9099982514

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...