Re: [MW:6597] pwht for service vessel

If it is service requirement you can not do welding for pressure to non pressure part also of any thickness.
 
please refer below extarct from ASME SEC VIII DIV 1- UCS 56.
 

The exemptions provided in Table

UCS-56 or Table UCS-56.1 are not permitted when postweld

heat treatment is a service requirement as set forth

in UCS-68, when welding ferritic materials greater than

18

in. (3 mm) thick with the electron beam welding process,

or when welding P-No. 3, P-No. 4, P-Nos. 5A, 5B, and

5C, P-No. 10, and P-No. 15E materials of any thickness

using the inertia and continuous drive friction welding

processes.

Regards
 
Asad

On Wed, Aug 18, 2010 at 7:19 AM, Karthik <karthik6684@yahoo.com> wrote:

Hi,

As per Code,Welding of pressure part cannot be done after PWHT.

But there is an option is that,you can weld the non pressure part to pressure part with fillet weld and the throat thickness should not exceed 13mm and also you have to do preheat with minimum 95 degree celcius,

If you meet the above criteria on your weld..you dont need to do PWHT again.


Thanks & Regards,


(Karthik)


Karthikeyan.S
 
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Wed, 8/18/10, sunilrathoreps@yahoo.com <sunilrathoreps@yahoo.com> wrote:

From: sunilrathoreps@yahoo.com <sunilrathoreps@yahoo.com>
Subject: [MW:6549] pwht for service vessel
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Date: Wednesday, August 18, 2010, 12:24 AM





Dear all

I have an vessel which is pwht as per service requirement,mention in note not to weld on pressure part after pwht cycle ,but we want cement lining inside the vessel up tp half portion to do this we have to put wire mash for lining to do this we have to weld this mesh with vessel , my  doubt is that is this required pwht ?even this mesh weld will nt be in contact with servic after lining . Vessel mat is kcs with 34mm thk.

Regards

Sunil singh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...