In practice, Travel speed for SMAW is about 5-15 mm/min. Current Type is DCEN or Electrode negative and for current is dependent to Electrode dia. and the position in welding. For example, if electrode dia. = 3 mm and position = vertical => current = 70-90 amp.
by

--- On Wed, 8/18/10, Raghuram Bathula <raghurambathula@gmail.com> wrote:

From: Raghuram Bathula <raghurambathula@gmail.com>
Subject: Re: [MW:6570] EA 981/15 electrdes
To: materials-welding@googlegroups.com
Date: Wednesday, August 18, 2010, 9:16 AM

http://www.elmics.ru/material/el/el0302_e.htm# (check the attachment)

On Wed, Aug 18, 2010 at 7:26 PM, mayur purwant <mayur15787@yahoo.co.in> wrote:
What Parameters (Current, Travel spee) should I used for EA981/15 electrodes.
 
 
Regards,
Mayur Purwant
Welding
Godrej & Boyce


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...