Re: [MW:6560] Conflict about heat available on electrode/work for the SMAW & GTAW process even having same polarity

Can you please elaborate for the benefit of whole group as all the people will not have the opportunity to look into the ASM handbook...seldom used at site.

Regards.
CK

On 18 August 2010 10:36, Kathalingam Babu <kathalingam.qaqc@ppl.com.sg> wrote:
Maulik,

It is not the conflict.

Pls understand the difference between the Thermionic & Non-Thermionic cathodes,

That will explains the heat distribution. Pls go through the topic of Arc Physics in ASM Welding Handbooks

Rgds,

K.Babu
Singapore


----- Original Message ----- From: "MAULIK" <mlkthakkar2@gmail.com>
To: "Materials & Welding" <materials-welding@googlegroups.com>
Cc: <bhavesh.patel@isgec.com>
Sent: Wednesday, August 18, 2010 1:47 AM
Subject: [MW:6549] Conflict about heat available on electrode/work for the SMAW & GTAW process even having same polarity



Dear all,


1. For SMAW-DCEN-2/3 heat to the electrode.

2. For GTAW-DCEN-2/3 heat to the work.


Why this is conflict?
Theoretically more heat is produced where the bombardment of electrons
is carried out.
Please give me clarification justification with proper evidence.

Regards,
Maulik H. Thakkar
Welding engineer



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...