Re: [MW:6547] FLUX

Hi,

yesterday i sent you about SAW fluxes for Inconel.


For normal fluxes please find below the details.


If fluxes comes with drums no need to baking before opening.

But if fluxes comes with bags,it shall be bake  to 300 - 350 degrees with 2hours to 10 hours.


Thanks & Regards,


(karthik)


Karthikeyan.S
 
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Tue, 8/17/10, Eng/ Mostafa Kamel Hussein <mkh_200@yahoo.com> wrote:

From: Eng/ Mostafa Kamel Hussein <mkh_200@yahoo.com>
Subject: [MW:6540] FLUX
To: materials-welding@googlegroups.com
Date: Tuesday, August 17, 2010, 3:29 PM

WHAT IS THE TEMPERATURE OF  HEATING OF FLUX IN SAW?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...