Hi,
 
Simulation heat treatment is performing on sample piece of material to be used in production.
If the production required PWHT for 2 Hrs, do PWHT in the sample piece of the material for three cycle. ie 6hrs. then carry out the tensile test and hardness test & if applicable impact also.
 
If any production repair required we have to confirm the property of material is safe after multiple PWHT.

Thanks & Regards
Muhammed Ibrahim PK



On 16 August 2010 23:06, asad azmi <azmiasadayub@gmail.com> wrote:
Dear All,
 
Greetings.
 
what is simulation  Treatment and where it is applicable.
 
 Please  expalin with example in reference to ASME SEC VIII DIV 1/ASME SEC II
 
Thanks in advance.
 
Regards
 
Asad 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...