Re: [MW:6495] but welding of unequal thickness member as per UW-9 OF ASME SEC VIII DIV 1

Taper has to be 1/3 with respect to the thickness difference. The width of the weld can be included in the taper.


  From: asad azmi [azmiasadayub@gmail.com]
  Sent: 14/08/2010 13:48 ZE3
  To: materials-welding@googlegroups.com
  Subject: [MW:6493] but welding of unequal thickness member as per UW-9 OF ASME SEC VIII DIV 1


Dear All,
 
Good Day.
 
 
 
Please  inform me what will be the Minimum length of the taper for butt weld between plates of 10 mm and 20mm Thickness.
 
Please refer Fig. 2 of the attachment and inform me--
 
whether length of taper will be distance between edge of plate ( The point from where tapering is statring ) to root face of the bevel i.e L
                                   OR 
Length of taper will be  from  edge of plate ( The point from where tapering is statring ) to the point where  thickness of the thicker member becomes equal to thickness of the thinner member i.e L1
 
What is the maximum angle allowed for tapering.( please refer Fig. 1(a)  of the attachment)
 
Thanks in advance.
 
Regards
 
Asad
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...