Thursday, August 12, 2010

Re: [MW:6470] Welder qualified

Dear Mr. Venkat
Good Day
 
Yes....Welder can weld....
As per QW-433 of ASME SEC. IX......F NO. 4 With and With out backing will qualify for F No. 1 With Backing for production. But its doesn't qualify F No. 1 with out backing.
And ofcourse...Welder is qualified for Welding of P1-P11,P34 & P41-P49 Materials.
M R Gupta
--- On Thu, 12/8/10, venkat ramana <venkatgps.ramana@gmail.com> wrote:

From: venkat ramana <venkatgps.ramana@gmail.com>
Subject: [MW:6466] Welder qualified
To: materials-welding@googlegroups.com
Date: Thursday, 12 August, 2010, 6:53 AM

Dear All,
 
Please let me know, my query is A welder was qualified with a P-1 test coupon using SMAW E7018 electrodes. May the welder weld P-4 material using E8028 electrodes with backing in production? (Assume the P-4 procedure using E8028 electrodes has been qualified)
 
Thanks & Regards
Venkat
 
 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...