Sunday, August 8, 2010

Re: [MW:6380] Re: BS EN-10204 3.1 & 3.2

Are we sure there is no catch here- The certification of supplier by his independent QA/
QC department.....? I think it has to be an independent 3rd party lab or similar.

--- On Sat, 7/8/10, JASPAL SINGH <jaspaldhesi@gmail.com> wrote:

From: JASPAL SINGH <jaspaldhesi@gmail.com>
Subject: [MW:0] Re: BS EN-10204 3.1 & 3.2
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Saturday, 7 August, 2010, 3:46 PM

BS EN-10204 3.1: The certification of supplier by his independent QA/
QC department.

Where as 3.2 is Witness of Testing required as per Technical Delivery
Conditions.

Regards

Jaspal Singh, CWI-AWS, CSWIP-3.1
Assistant Manager – Quality Assurance
Process Equipment Division
ISGEC, Yamuna Nagar, Haryana -135001
Phone: 911732307251
Ext: 251 Mb: +918930111441

"To love what you do and feel that it matters - how could anything be
more fun?"



On Aug 7, 2:31 pm, Noushad cp <ncp....@gmail.com> wrote:
> Dear All,
>
> I would like to know the diffrence between 3.1 and 3.2 Certification.
>
> Please explain in detail way.Applicable test and all.
>
> Regards,
>
> NCPTesting

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...