     First is 2.2 - material manufacturer cert.
     Second is 3.1 - manufacturer cert cum the buyer QC witnessing & certifying the matl.
     Third is 3.2 - the licencse TPI (DNV,LLoyds, ABS etccccc) witnessing & certifying the material.
 
 
Rgds,
P.Mahendran

--- On Sat, 7/8/10, B.Vaithiyanathan <pavainathan@gmail.com> wrote:

From: B.Vaithiyanathan <pavainathan@gmail.com>
Subject: Re: [MW:6364] BS EN-10204 3.1 & 3.2
To: materials-welding@googlegroups.com
Date: Saturday, 7 August, 2010, 6:04 PM

In 3.1 certification Manufacturer and his quality will certify the material
in case of 3.2 certification Purchaser or TPI witness and certification of material is required.
 
Vaithiyanathan,
Oman

On Sat, Aug 7, 2010 at 1:31 PM, Noushad cp <ncp.clt@gmail.com> wrote:
Dear All,
 
 
I would like to know the diffrence between 3.1 and 3.2 Certification.
 
Please explain in detail way.Applicable test and all.
 
 
 
Regards,
 
NCP
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
With Best Regards

B.Vaithiyanathan
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...