Saturday, August 7, 2010

Re: [MW:6358] Hydrotesting of pipeline

for safety point of view and for the confirmation of the weld quality you can adopet the any NDT method according to the requirement like RT having the record and UT no record  ( RT and UT  can check the quality of complete weld ) and DPT is only for the surface defect.
 
it will be advicable to have the RT and DPT test for the weld of header rest depand on the procedure or specification.

On 7 August 2010 12:42, sumit jaura <sumit.jaura@gmail.com> wrote:
Dear all,

Can anyone suggest that whether it is must to have radiography of all
flanges and nipples on test header for hydrotesting?

or we can only allow by ut or dpt only.

Sumit ,

P. engineer,

Worleyparsons

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Regards

Rajeev Arora




"DON'T LET SOMEONE BECOME A PRIORITY IN YOUR LIFE...
WHEN YOU ARE JUST AN OPTION FOR THEM....."

 SO , Always keep in mind that......

DON'T GO THE WAY LIFE TAKES YOU,
TAKE THE LIFE THE WAY YOU GO,

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...