Dear all,
yes, what mr.ajay said is correct. My experience, during the welding they should not use the grinding whell/cutting whell for cleaning or correct the welding. They use stainless steel wire brush for cleaing during the time of welding (if it is required)
Preheat, it is need before weld as per WPS.
Weather shilding is must. (weld booth)
Check the Argon purity.
regards
spsamy
On Thu, Aug 5, 2010 at 11:09 PM, kcrtechnical <kcrtechnical@gmail.com> wrote:
Dear All,What are all the probable reasons for getting porosity in aluminium welding, other than weather conditions, here both material and filler are 99.7% Pure Aluminium.Please share with any type of reason.K C R--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment