Re: [MW:6333] Power boiler repair before start up

If boiler already certified (stamped and all MDRs including those for assembly signed) then you must involve NB R stamp holder. If not yet certified then you open an NCR and you repair provided you are at least ASME R stamp holder


----- Original Message -----
From: limesh M [limesh78@gmail.com]
Sent: 05/08/2010 23:07 MST
To: "Materials & Welding" <materials-welding@googlegroups.com>
Subject: [MW:6330] Power boiler repair before start up

Dear All,

One of the boiler's burner front wall tubes found corroded.Boiler is
new one and not yet commissioned.Boiler assembled by us.Can I use my
company's or hired welders for a boiler repair constructed by other
company? ASME Authorised Inspector denied our request to utilise our
welders.AI advised us to bring the welders from the manufacturer side
for repair.Which code clause justifying his comment?

Regards,


Limesh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...