Dear all

I have an vessel which is pwht as per service requirement,mention in note not to weld on pressure part after pwht cycle ,but we want cement lining inside the vessel up tp half portion to do this we have to put wire mash for lining to do this we have to weld this mesh with vessel , my doubt is that is this required pwht ?even this mesh weld will nt be in contact with servic after lining . Vessel mat is kcs with 34mm thk.

Regards

Sunil singh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...