Thursday, August 12, 2010

[MW:6458] P42 (Monel) to P1 (SA516 G.70) Welding

Gents,
 
We have to weld a monel Nozzle SB165 (UNS N04400) (P No.42) to SA516G.70 (PNo.1) 45 mm thk
 
The vessel is required PWHT.
 
I need to qualify a PQR for this welding with ERNiCu+ENiCu-7.
 
Is it required to do PWHT of this joint (P42 to P1)?.
 
If PWHT is required what is the way of  welding of this joint?
 
If  PWHT is not required what is the procedure to weld it?
 
Is it required to butter the CS with monel before butt welding?
 
Is any post heting is required for this joint?
 

Thanks & Regards
Muhammed Ibrahim PK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...