We got one WPS/PQR as below
Base metal ASTM A351 Gr.CK3MCun.
Filler metal :SFA 5.11 F.NO 43 A.NO.9 E Ni Cr Mo3
The above base & filler metal is one WPS/PQR
The second WPS/PQR is given as below
Base metal: ASTM A351 Gr.CK3MCun
Filler metal:SFA 5.11 ASTM A351 20Cr 18Ni 6Mo F.NO 43 A.NO 9
Is it acceptable by giving as Filler metal:ASTM A351 20Cr 18Ni 6Mo F.NO 43 A.NO 9 in the WPS/PQR & WELDER ID CARD instead of giving the AWS Classification.
Thanks,
kk
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
We got one WPS/PQR as below
Base metal ASTM A351 Gr.CK3MCun.
Filler metal :SFA 5.11 F.NO 43 A.NO.9 E Ni Cr Mo3
The above base & filler metal is one WPS/PQR
The second WPS/PQR is given as below
Base metal: ASTM A351 Gr.CK3MCun
Filler metal:SFA 5.11 ASTM A351 20Cr 18Ni 6Mo F.NO 43 A.NO 9
Is it acceptable by giving as Filler metal:ASTM A351 20Cr 18Ni 6Mo F.NO 43 A.NO 9 in the WPS/PQR & WELDER ID CARD instead of giving the AWS Classification.
Thanks,
kk
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments