Monday, August 2, 2010

[MW:6250] clad welding

I have to weld SA516 Gr 70 which has a 410 clad backing has anybody
done this? if so how were the results, there is no PWHT involved. 25mm
thick plate for a pressure vessle.
I have to qualify a PQR would be interested to read all comments

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...