Re: [MW:4253] Fillet weld qualification in 2F position for SAW process.

You can increase the thickness of the base material.
Please check the General Note at the bottom of QW-452.5 , i.e. production mockup test.
 
Regards,

On Tue, Jan 26, 2010 at 7:09 PM, PAMULA <vasantharao2009@rediffmail.com> wrote:


Dear All,

I have a requirement to qualify a welder in 2F position for SAW process.

I have referred the test requirement in QW 542.5 of ASME Sec.IX.

For fillet weld qualification, test coupon thickness is given up to 10 mm only.

For SAW Qualification in 2F, shall i use plate thickness higher than 10mm?

Is there any reference/limitations for plate thickness in Sec.IX?

Pl. provide your valuable suggestions.

regards
P.Rao




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Sukamal

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...