Tuesday, February 2, 2010

[MW:4176] Impact Tested PQR for Non Impact Tested WPS

Dear All,

Note-1:A PQR was Impact tested at -46 C, on a 12" Dia Pipe Sch 40 (Wall Thickness=10.31mm) Deposited Weld Metal: GTAW=4mm & Balance SMAW.
Note-2: The WPS Supported by Above PQR is not Impact tested Designed Welding.

Q: Can this Impact Tested PQR support a non Impact Tested WPS which is to be used for Welding of D-catagory(B31.3-300.2) Piping.(Non LTCS).
Q: What will be the ranges of qualification of deposited metal & base metal.
Q If we want to make two WPSs from this PQR (1- for GTAW for Small Thickness Welding & 2- for GTAW/SMAW for larger thickness). What to do?

Any code case, ASME IX interpretation or reference that we can refer to.

Regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35346] Cast-iron welding

Any advice for cast iron welding Sent from Yahoo Mail for iPhone