Skip to main content

RE: [MW:3748] ASME B31.3 unlisted materials

In general : check requirements towards weld metal for AISI 4130 joints : strength , hardness, charpy values

In oil industry you can have requirements for high strength where B2 will fail.

In oil industry you will have probably Nace requirements (max 22HRC) : you will need high PWHT temp to reduce HAZ hardness.

Chary values at -46degrC ..?

 

AISI 4130 base metal can be ordered and supplied with high strength levels.

 

With kind regards,

Erwin GERING

 

Van: pgoswami@sympatico.ca [mailto:pgoswami@sympatico.ca]
Verzonden: dinsdag 24 november 2009 23:29
Aan: materials-welding@googlegroups.com
Onderwerp: FW: [MW:3727] ASME B31.3 unlisted materials

 

 

 Hi John,

 

I have attached a spec for 4130 steel FYI. The summarized details are as follows:-

§                ASTM 519 Gr 4130—Nearest ASME Sec IX P No- 4. (typically 1.00- 1.25 Cr, 0.5% Mo)

§                Welding  Consumables–SMAW –E-8018 B2 or 7018-B2L , GTAW-ER-80S-B2

§                PWHT—Follow PWHT requirements for P4 materials as asked by B 31.1 code (Table 331.1.1).

§                Recommended PWHT cycle should be , Soaking Temp-1300-13750F, Soaking Time -1 Hr/inch of thickness, Minimum soak time –1 hr

§                Targeted hardness 225 BHN Max.

 

Since this material is not listed in B-31.3, proper design evaluation, stress analysis (if required) should be done prior to use. Follow the guidelines of B-31.13 code for the same.

 

You may find the guidelines of ASME 31.3 code on the use of unlisted materials, as mentioned below.

 

Hope this would be of help to you.

 

Thanks.

 

Pradip Goswami,P.Eng

Senior Engineer/Specialist(Welding-Metallurgy)

Machine Dynamics & Component Integrity Dept.

Engineering & Training Services Division

ONTARIO POWER GENERATION Inc.

PO Box-2000, RR-55(South)

Nanticoke, Ontario,N0A1L0

Tel:-(519) 587-2201, Ext 3107--in Nanticoke

         (416) 231-4111, Ext 5925--in Kipling,Toronto

Fax: (519) 587-6814

Email-pradip.goswami@opg.com.

 

Unlisted Materials. Unlisted materials may be used provided they conform to a published specification covering chemistry, physical and mechanical properties,

method and process of manufacture, heat treatment, and quality control, and otherwise meet the requirements of this Code. Allowable stresses shall be determined in accordance with the applicable allowable stress basis of this Code or a more conservative basis.

 

Unlisted  Materials.  An unlisted material, shall be qualified for service at all temperatures within a stated range, from design minimum temperature to design maximum temperature.

 

 

From: j.lock@pacificdrilling.com
To: materials-welding@googlegroups.com
Date: Mon, 23 Nov 2009 15:27:23 -0800
Subject: RE: [MW:3717] ASME B31.3 unlisted materials

The material is ASTM 519 Gr 4130

 

Best regards,

 

John Lock

Quality & Classification Engineer

Pacific Deepwater Construction Ltd

cid:image002.jpg@01CA4F2E.75D71400

Cellular.                 +82 (0)10 4693 6282

Office Tel.              +82 (0)55 631 9071

Office Fax.             +82 (0) 631 7499

E-mail                    j.lock@pacificdrilling.com

P Before printing I think about the environment

 

From: pgoswami@sympatico.ca [mailto:pgoswami@sympatico.ca]
Sent: Friday, November 20, 2009 10:08 PM
To: materials-welding@googlegroups.com
Subject: RE: [MW:3705] ASME B31.3 unlisted materials

 

What is the unlisted material, could you be specific, i.e. could you please provide specification or composition etc.
 
Thanks.
 
Pradip Goswami,P.Eng
Welding & Metallurgical Engineer/Specialist.
Ontario Power Generation Inc.
Toronto, Canada.
 
> Date: Thu, 19 Nov 2009 23:43:10 -0800
> Subject: [MW:3695] ASME B31.3 unlisted materials
> From: jjlock53@gmail.com
> To: materials-welding@googlegroups.com
>
> Should PWHT requirements for the materials type be followed for
> unlisted materials i.e. no P or S number?
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



THIS MESSAGE IS ONLY INTENDED FOR THE USE OF THE INTENDED RECIPIENT(S) AND MAY CONTAIN INFORMATION THAT IS PRIVILEGED, PROPRIETARY AND/OR CONFIDENTIAL. If you are not the intended recipient, you are hereby notified that any review, retransmission, dissemination, distribution, copying, conversion to hard copy or other use of this communication is strictly prohibited. If you are not the intended recipient and have received this message in error, please notify me by return e-mail and delete this message from your system. Ontario Power Generation Inc.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...