Re: [MW:3765] Torque calculation

Torque,in lb.ft=KDP/12
 
K=0.2 for finished bolts;0.22 for Zn Plated;0.3 for black;0.16 for Cd plated;0.15 to 0.18 for lubricated;0.10 for highly lubricated or waxed

D=nominal dia of bolt in inches
P=Bolt's desired load in Lbs(=75% of YSXArea)
A,area=0.7854X Square of (D - 0.9743/n)
n=no of threads pre inch;
Coarse series(UNC) 1/2=13
                              5/8=11
                              3/4=10
                              7/8=09
8UN series 1" onwards=8
Hope above information shall help
Regards
Aarpee
On Sun, Nov 29, 2009 at 11:45 AM, Mrityunjay Kumar / ZS Saudi PEB QA/QC <Mrityunjaykumar@zamilsteel.com> wrote:

Hi,

Good morning,

Can anybody tell me the formulae for Torque calculation (if load & area is provided for Anchor Bolts).

 

 

 Thanks and Regards,

M.K.Choudhary

--------------------------------------------------------------------------------------------------------
Disclaimer: This email and any files transmitted with it are confidential
and intended solely for the use of the addressee(s) named herein. If you
are not the intended recipient or addressee, you should not use, disseminate,
distribute, copy or alter this email. Any views or opinions presented in this
email are solely those of the author and might not represent those of "Zamil
Industrial" and or its units.

Warning: Although reasonable precautions have been taken to ensure no viruses
are present in this email, the company cannot accept responsibility for any
loss or damage arising from the use of this email or attachments. If you have
received this electronic mail message in error, please contact the sender directly.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...